ACI 207.2R-1995

Effect of Restraint, Volume Change, and Reinforcement on Cracking of Mass Concrete


 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 ACI 207.2R-1995 前三页,或者稍后再访问。

如果您需要购买此标准的全文,请联系:

点击下载后,生成下载文件时间比较长,请耐心等待......

 

标准号
ACI 207.2R-1995
发布日期
1995年03月
实施日期
废止日期
发布单位
美国混凝土学会
适用范围
This report is primarily concerned with limiting the width of cracks in structural members that occur principally from restraint of thermal contraction. A detailed discussion of the effects of heat generation and volume changes on the design and behavior of mass reinforced concrete elements and structures is presented. It is written primarily to provide guidance for the selection of concrete materials, mix require?ments, reinforcement requirements, and construction proce?dures necessary to control the size and spacing of cracks. Particular emphasis is placed on the effect of restraint to vol?ume change in both preventing and causing cracking and the need for controlling peak concrete temperature. The quality of concrete for resistance to weathering is not emphasized in recommending reduced cements contents; however, it should be understood that the concrete should be sufficiently durable to resist expected service conditions. The report can be applied to any concrete structure with a potential for un?acceptable cracking; however, its general application is to massive concrete members 18 in. or more in thickness.

ACI 207.2R-1995相似标准





Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号