适用范围
This specification covers the requirements for four types of welded austenitic stainless steel tube of outside diameter not exceeding 57 mm, each type being subdivided into Class A (general engineering purpose tube) and Class B (low pressure hydraulic tube). NOTE a) The titles of standards referred to by number in the specification are given in Appendix A. b) Requirements that must be specified by the purchaser and those that must be agreed upon are listed in Appendix B. c) A table of non-metric sizes of welded Austenitic stainless steel tube (to be retained only while non-metric units are still in use) is given in Appendix C. ^Conversion factors are given in Appendix D.

SANS 965:1969相似标准


推荐

新莱 | 坚守高标准制管工艺

上文和大家诠释了为什么表面光亮度≠表面粗糙度,这次就来解答下客户疑问—“为什么别人管道比新莱看起来更光亮”。在线光亮固溶处理为什么要固溶处理不锈钢管在生产过程中因为遭受滚压、拉伸与焊接高温影响,使材料组织、机械性能均会产生变化,影响不锈钢管质量:01金相不良制管时,母材受焊接形成热影响区,其内部各相组织形态各异:铁素体、马氏体、奥氏体等其他金相组织,极大影响管道耐腐蚀性。...

304、304L、316、316L区别在哪?这到底是不锈钢还是不锈铁?

为获得最佳耐腐蚀性能,316不锈钢钢焊接断面需要进行焊后退火处理。如果使用316L不锈钢,不需要进行焊后退火处理。   机械性能在所有钢材中,奥氏体不锈钢屈服点最低。因此从机械性能考虑,奥氏体不锈钢并不是用在阀杆最佳材料,因为要保证一定强度,阀杆直径就会加大。屈服点不能通过热处理来提高,但可以通过冷成型提高。   ...

乳品、焊接,原来是这样关系

有些焊接氧化非常严重,已经破坏奥氏体不锈钢本体材质耐腐性、光洁度,易出现滋生细菌、抗腐蚀下降结果,这就是一个很严重质量风险点,因为这里永远隐藏着细菌,不断滋生细菌会影响很多批次产品。图9 焊缝未熔透等失败案例04焊接不合格导致细菌滋生等问题图10 焊口中容易存在李斯特菌、沙门氏菌在焊接不合格位置,李斯特菌、沙门氏菌在反复污染着我们产品。...

岛津EPMA超轻元素分析之五: 局部N元素富集造成不锈钢管微裂纹?

2N元素在不锈钢中作用元素N是双相不锈钢中有益元素,双相不锈钢强度和耐蚀性能因为N元素合金化作用而表现更为优异。N可以扩大钢奥氏体相区,是一种很强形成和稳定奥氏体元素,其效力约是镍20倍,在一定限度内可代替部分昂贵Ni。3不锈钢管中N元素电子探针测试某采用双相不锈钢制作换热器管件,在用胀管工艺实现管束和管板连接时发生换热管管壁胀裂现象。...