SAE AS7454C-2018
螺栓和螺钉 钢 低合金 耐热 135 000 psi 抗拉强度 正火和回火 滚制螺纹

Bolts and Screws@ Steel@ Low Alloy@ Heat Resistant 135@000 psi Tensile Strength@ Normalized and Tempered@ Roll Threaded


标准号
SAE AS7454C-2018
发布
2018年
发布单位
SAE - SAE International
当前最新
SAE AS7454C-2018
 
 
适用范围
Type This procurement specification covers aircraft quality bolts and screws made from a low alloy@ heat resistant steel of the type identified under the Unified Numbering System as UNS K14675. AS7454 135000 psi ultimate tensile strength at room temperature. AS7454-1 135000 psi ultimate tensile strength at room temperature@ nickel-cadmium plated. Application Primarily for aerospace propulsion system applications where good strength at temperatures up to approximately 900 ??is required and the part is protected against corrosion. Safety - Hazardous Materials While the materials@ methods@ applications@ and processes described or referenced in this specification may involve the use of hazardous materials@ this specification does not address the hazards which may be involved in such use. It is the sole responsibility of the user to ensure familiarity with the safe and proper use of any hazardous materials and to take necessary precautionary measures to ensure the health and safety of all personnel involved. Usage of Existing Manufactured Stock. Unless otherwise specified@ part inventory manufactured to previous revisions of this specification may be procured and used until stock is depleted.

SAE AS7454C-2018相似标准


推荐

合金元素在中的作用

钴能强化铁素体,加入碳素中,在退火或正火状态下能提高的硬度、屈服点抗拉强度,对伸长率断面收缩率有不利的影响,冲击韧性也随着钴含量的增加而降低。由于钴具有抗氧化性能,在耐热耐热合金中得到应用。钴基合金燃气涡轮中更显示了它特有的作用。(10)硅(Si)硅能溶于铁素体奥氏体中提高的硬度强度,其作用仅次于磷,较锰、镍、铬、钨、钼、钒等元素强。但含硅量超过3%时,将显著降低的塑性韧性。...

中各元素的作用

碳(C)中含碳量增加,屈服点抗拉强度升高,但塑性冲击性降低,当碳量0.23%超过时,的焊接性能变坏,因此用于焊接的低合金结构,含碳量一般不超过 0.20%。碳量高还会降低的耐大气腐蚀能力,在露天料场的高碳钢就易锈蚀;此外,碳能增加的冷脆性时效敏感性。铬(Cr)铬能增加的淬透性并有二次硬化的作用,可提高碳钢的硬度耐磨性而不使变脆。...

冬天里的四把火!!!!

组织:回火索氏体组织(由等轴状 α相粒状渗碳体组成的机械混合物)性能:具备良好的综合机械性能(较高的强度、塑性、韧性)。适用钢种:中碳结构低合金钢应用:适用于重要机器零件,如发动机曲轴、连杆、连杆螺栓、汽车拖拉机半轴、机床主轴及齿轮等。这些零件在使用中要求较高的强度并能承受冲击交变载荷的作用。(28≤HRC≤33)5.小结...

【材料课堂】热处理特辑—回火

回火后得到回火索氏体,指马氏体回火时形成的铁素体基体内分布着细小球状碳化物(包括渗碳体)的复相组织。力学性能:25~35HRC,较好的综合力学性能。应用范围:广泛用于各种较重要的受力结构件,如连杆、螺栓、齿轮及轴类零件等。工件淬火并高温回火的复合热处理工艺称为调质。调质不仅作最终热处理,也可作一些精密零件或感应淬火件预先热处理。45正火调质后性能比较见下表所示。...