This specification covers a titanium alloy in the form of bars, wire, forgings, flash welded rings, and stock for forging or flash welded rings. These products have been used typically for parts requiring high strength- to-weight ratio up to 750 degrees F (399 degrees C), but usage is not limited to such applications. Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; SAE ARP 982 recommends practices to minimize such conditions.
SAE AMS 4979E-2003由美国机动车工程师协会 US-SAE 发布于 2003-06-01。
SAE AMS 4979E-2003 在中国标准分类中归属于: V11 航空与航天用金属铸锻材料,H64 稀有轻金属及其合金,在国际标准分类中归属于: 49.025.30 钛。
SAE AMS 4979E-2003 6A1 6V 2Sn经固溶热处理和沉淀硬化处理过的钛合金棒材、线材、锻件和环 于 2008-01-01 变更为 SAE AMS 4979F-2008 6A1 6V 2Sn溶解和沉淀热处理的钛合金棒材、线材、锻件和环材。