AWS B2.1-22-015-2002
带或不带支持网页执照,在焊接条件下18到10计,(M/P/S-22到M/P/S-22)铝钨板气体保护焊的标准焊接程序规范

Standard Welding Procedure Specification (WPS) for Gas Tungsten Arc Welding of Aluminum, (M/P/S-22 TO M/P/S-22), 18 Through 10 Gauge, in the As-Welded Condition, with or without Backing Site License [Superseded: AWS B2.1-1-015]


 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 AWS B2.1-22-015-2002 前三页,或者稍后再访问。

您也可以尝试购买此标准,
点击右侧 “购买” 按钮开始采购(由第三方提供)。

点击下载后,生成下载文件时间比较长,请耐心等待......

 

标准号
AWS B2.1-22-015-2002
发布
2002年
发布单位
美国焊接协会
替代标准
AWS B2.1-22-015-2011
当前最新
AWS B2.1-22-015-2011
 
 
适用范围
This Standard WPS is to be used only as permitted by the applicable fabrication document( s); such as code, specification, or contract document(s). The fabrication document(s) should specify the engineering requirements such as design, need for heat treatment, fabricating tolerances, quality control, and examination and tests applicable to the end product.

AWS B2.1-22-015-2002相似标准


推荐

半导体专业术语含义

170. silicon on sapphire(SOS)epitaxial wafer:外延是蓝宝石衬底硅原片171. small scale integration(SSI):小规模综合,单一模块上由210个图案布局。172. source code:原代码,机器代码编译者使用,输入程序设计语言里编码器代码。...

福建省特检院预算442万采购多功能数显卡尺等仪器设备

,可确保至少1050℃条件下连续工作2)类型:K型;焊接点需位于铠装套内;3)热电偶允差应符合GB/T 16839.2-19971级标准:0-375℃允差:±1.5℃;375~750℃允差:±0.004*|t|18002-3A033499-其他专用仪器仪表功率分析仪1(台)否1.电压量程:0.5~600V;电压精度:±1%;2.电流量程:0.05mA~20A;电流精度:±1%;3.测试带宽:DC...

【材料课堂】铝合金焊接方法和材料选用

厚为25~50㎜时,采用添加10%~35%ArAr+He混合气体。当厚为50~75㎜时,宜采用添加10%~35%50%HeAr+He混合气体。当厚>75㎜时,推荐添加50%~75%HeAr+He混合气体。 铝合金焊接工艺1  铝合金气焊氧-乙炔气焊热效率低,焊接热输入不集中,焊接及铝合金时需采用熔剂,后又需清除残渣,接头质量及性能也不高。...

【材料课堂】铝合金焊接关键技术

由于焊接方法及焊接工艺参数选取不当,造成铝合金零件焊接后产生严重变形,因为焊缝气孔、夹渣、未透等缺陷,导致焊缝金属裂纹材质疏松,严重影响了产品质量及性能。以下小编就您分析铝合金焊接方法以及注意事项。 铝合金三种焊接方法 极氩弧焊 极氩弧焊法主要用于铝合金,是一种较好焊接方法,不过极氩弧焊设备较复杂,不合适露天条件下操作。 ...