SAE AMS 5663L-2003
UNS N0 在1,775℉(968℃)下自耗电极或真空感应熔炼并经脱溶热处理的含52.5Ni-19Cr-3.0Mo-5.1Cb-0.90Ti-0.50Al-18Fe耐腐蚀耐热镍合金棒,锻件和环件

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution and Precipitation Heat Treated UNS N0


SAE AMS 5663L-2003 发布历史

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars,forgings,flash welded rings,and stock for forging or flash welded rings.These products have been used typically for parts requiring high resistance to creep and stress-rupture up to 1300℉(704℃)and oxidation resistance up to 1800℉(982℃),but usage is not limited to such applications.

SAE AMS 5663L-2003由美国机动车工程师协会 US-SAE 发布于 2003-07-01。

SAE AMS 5663L-2003 在中国标准分类中归属于: V11 航空与航天用金属铸锻材料。

SAE AMS 5663L-2003的历代版本如下:

  • 2003年07月01日 SAE AMS 5663L-2003 UNS N0 在1,775℉(968℃)下自耗电极或真空感应熔炼并经脱溶热处理的含52.5Ni-19Cr-3.0Mo-5.1Cb-0.90Ti-0.50Al-18Fe耐腐蚀耐热镍合金棒,锻件和环件

SAE AMS 5663L-2003 UNS N0 在1,775℉(968℃)下自耗电极或真空感应熔炼并经脱溶热处理的含52.5Ni-19Cr-3.0Mo-5.1Cb-0.90Ti-0.50Al-18Fe耐腐蚀耐热镍合金棒,锻件和环件 于 2004-07-12 变更为 SAE AMS 5663M-2004 经1775℉(968℃)溶液和沉淀热处理以及熔化电极或真空感应熔化的52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 19Fe耐腐蚀和耐热镍合金条材、锻材和环材。

 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 SAE AMS 5663L-2003 前三页,或者稍后再访问。

点击下载后,生成下载文件时间比较长,请耐心等待......

 



标准号
SAE AMS 5663L-2003
发布日期
2003年07月01日
实施日期
废止日期
中国标准分类号
V11
发布单位
US-SAE
代替标准
SAE AMS 5663M-2004
适用范围
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars,forgings,flash welded rings,and stock for forging or flash welded rings.These products have been used typically for parts requiring high resistance to creep and stress-rupture up to 1300℉(704℃)and oxidation resistance up to 1800℉(982℃),but usage is not limited to such applications.




Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号