This European Standard is one of a series dealing with products and systems for the protection and repair of concrete structures. It specifies a method for determining the loss of mass after freeze-thaw salt stress in sodium chloride solution. It can be used to test the resistance of hydrophobic impregnated concrete as well as the untreated concrete. There are two types of concrete deterioration when a freeze-thaw attack occurs: surface scaling and internal damage.

DIN EN 13581-2002由德国标准化学会 DE-DIN 发布于 2002-12。

DIN EN 13581-2002 在中国标准分类中归属于: P97 建筑工程施工机械,在国际标准分类中归属于: 91.080.40 混凝土结构。

DIN EN 13581-2002的历代版本如下:

  • 2002年12月 DIN EN 13581-2002 混凝土构件的保护和检修用产品和系统.试验方法.盐力解冻后疏水性浸渍混凝土质量损失的测定; 德文版本 EN 13581:2002

 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 DIN EN 13581-2002 前三页,或者稍后再访问。

点击下载后,生成下载文件时间比较长,请耐心等待......

 



标准号
DIN EN 13581-2002
发布日期
2002年12月
实施日期
废止日期
中国标准分类号
P97
国际标准分类号
91.080.40
发布单位
DE-DIN
被代替标准
DIN EN 13581-1999
适用范围
This European Standard is one of a series dealing with products and systems for the protection and repair of concrete structures. It specifies a method for determining the loss of mass after freeze-thaw salt stress in sodium chloride solution. It can be used to test the resistance of hydrophobic impregnated concrete as well as the untreated concrete. There are two types of concrete deterioration when a freeze-thaw attack occurs: surface scaling and internal damage.