SIS SS IEC 474:1986
绝缘油.加抑制剂的矿物绝缘油氧化稳定性检测方法

Insula t ing oils — Test method for oxidation stability of inhibited mineral insula ting oils


 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 SIS SS IEC 474:1986 前三页,或者稍后再访问。

您也可以尝试购买此标准,
点击右侧 “购买” 按钮开始采购(由第三方提供)。

点击下载后,生成下载文件时间比较长,请耐心等待......

 

标准号
SIS SS IEC 474:1986
发布
1986年
发布单位
SE-SIS
当前最新
SIS SS IEC 474:1986
 
 
适用范围
This publication describes a test for the oxidation stability of unused inhibited mineral insulating oils by measure-ment of the induction period. This method may also be used to obtain information on the acid- and sludge-forming tendency before or after the induction period. The method is only intended for testing the continuity of oil supplies. The results do not necessarily provide information of the performance in .service.

SIS SS IEC 474:1986相似标准


推荐

高压差式扫描量热仪(HPDSC)评价润滑油氧化安定性

评价润滑油氧化安定性方法GB/T 12580-1990 抑制剂矿物绝缘油氧化安定性测定法NB/SH/T 0811-2010 未使用过烃类绝缘油氧化安定性测定法SH/T 0124-2000 含抗氧剂汽轮机油氧化安定性测定法SH/T 0185-1992 直馏润滑油氧化安定性测定法SH/T 0193-2008 润滑油氧化安定性测定.旋转氧弹法以上这些方法基本上都是油品在空气或者氧气和金属催化剂环境中恒温氧化一定时间...

气相色谱仪检测矿物绝缘油中二苄基二硫醚含量

矿物绝缘油是从石油中提炼精制液体绝缘材料,简称矿物油。石油主要成分是烷烃、环烷烃和芳香烃,这些组分电气性能和老化稳定性优良。环烷基原油因含蜡量较少,可用来制造低凝固点绝缘油,又因含芳香烃组分较多,在电场作用下不但不析出气体,还吸附气体,故多以它制造绝缘油。环烷基原油在世界上储量少,现正研究以石蜡基原油制造绝缘油。原油中还含有树脂质、沥青质及少量氧、氮、硫等元素化合物。...

红外光谱法在矿物绝缘油润滑油结构族组成测定上应用

摘要: 矿物油是指从石油中提炼精制液体绝缘材料。石油主要成分是烷烃、环烷烃和芳香烃,这些组分电气性能和老化稳定性优良。根据具体用途适当控制各组分含量,可以得到变压器油、开关油等绝缘油以及各种润滑油。例如,芳香烃成分可有效吸附气体可用于制作电缆油或电容器油、环烷烃成分可以降低油份凝固点用于制作低温润滑油。...

油分析仪器 | 全自动体积电阻率测定仪

液体内部直流电场强度与稳态电流密度商称为液体介质体积电阻率,它是判断油品老化及污染程度重要指标,体积电阻率对油离子传导损耗反应灵敏,不论是酸性或中性氧化物,都能引起电阻率明显变化,所以通过对体积电阻率测定,能可靠有效监督油质运行情况。...