DIN EN ISO 12732-2008
金属和合金的腐蚀.使用双环法测量电化学电动势活化(基于Cihal法)

Corrosion of metals and alloys - Electrochemical potentiokinetic reactivation measurement using the double loop method (based on Cihal's method) (ISO 12732:2006); German version EN ISO 12732:2008


 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 DIN EN ISO 12732-2008 前三页,或者稍后再访问。

如果您需要购买此标准的全文,请联系:

点击下载后,生成下载文件时间比较长,请耐心等待......

 

标准号
DIN EN ISO 12732-2008
发布日期
2008年07月01日
实施日期
废止日期
中国标准分类号
H25
国际标准分类号
77.060
发布单位
DE-DIN
引用标准
ISO 8044-1999 ISO 643-2003
适用范围
This International Standard specifies the method for measuring the degree of sensitization (DOS) in stainless steel and nickel-based alloys using the Double Loop Electrochemical Potentiokinetic Reactivation (DL-EPR) test (based on (~ihal's method). The method may be used for the quantitative assessment of deleterious thermal effects resulting in the formation of alloy-element-depleted zones at grain boundaries or in the matrix. However, attention should be paid when testing heat-affected weld zones, due to possible non-uniform distribution of sensitized zones along the fusion lines. The results of the test can be used as an index to identify the potential susceptibility of stainless steel and nickel-based alloys to intergranular corrosion, pitting corrosion, and intergranular-stress corrosion cracking, but prediction of these corrosion modes depends on complementary specific testing. This International Standard describes the general methodology and, in Annex C, gives examples of suitable test exposure conditions for specific alloys.




Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号