ASTM D6442-1999
海水中防污涂料系统的铜释放率的标准试验方法

Standard Test Method for Copper Release Rates of Antifouling Coating Systems in Seawater


说明:

  • 此图仅显示与当前标准最近的5级引用;
  • 鼠标放置在图上可以看到标题编号;
  • 此图可以通过鼠标滚轮放大或者缩小;
  • 表示标准的节点,可以拖动;
  • 绿色表示标准:ASTM D6442-1999 , 绿色、红色表示本平台存在此标准,您可以下载或者购买,灰色表示平台不存在此标准;
  • 箭头终点方向的标准引用了起点方向的标准。

 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 ASTM D6442-1999 前三页,或者稍后再访问。

点击下载后,生成下载文件时间比较长,请耐心等待......

 



标准号
ASTM D6442-1999
发布日期
1999年
实施日期
废止日期
中国标准分类号
Z16
国际标准分类号
87.040 (Paints and varnishes)
发布单位
US-ASTM
适用范围

1.1 This test method covers the laboratory determination of the rate at which copper is released from an antifouling coating in synthetic seawater using graphite furnace atomic absorption spectrophotometry (GF-AAS).

1.2 The procedure contains the preparation steps for the leach rate determination of copper from antifouling paints including apparatus, reagents, holding tank conditions, and sampling point details. Analysis for the concentration of copper in seawater requires the accurate determination of copper at the low parts per billion (ppb) level. To detect and correct for reagent impurities, acceptable analytical precision standards are necessary. Therefore, the limit of quantitation for the analytical method should be 6 ppb or less. The method of choice for most commonly available instrument with the greatest sensitivity would be GF-AAS. This procedure is written to include necessary steps to isolate the copper from seawater, thereby increasing sensitivity and eliminating salts that interfere with the use of atomic absorption techniques.

1.3 Other analytical methods may be utilized with appropriate procedural changes, as needed, to accommodate selectd specific methods. Such methods must meet the limit of quantition (6 ppb) as presented in Section

1.4 This test method has not yet been validated to reflect in-situ copper release rates for antifouling products and therefore should not, at present, be used in the process of generating environmental risk assessments. In-service release rates of antifouling (AF) coatings are expected to vary with natural variability in seawater chemistry, temperature, and hydrodynamic regime.

1.5 The values stated in SI units are to be regarded as standard. The inch-pound units given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety practices and to determine the applicability of regulatory limits prior to use. For specific hazard statements, see Section .