BS EN 12513-2011
铸造.铸铁耐磨性

Founding. Abrasion resistant cast irons


BS EN 12513-2011 发布历史

This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of:  chemical composition;  hardness. The types of abrasion resistant white cast irons covered by this standard are: a) unalloyed or low alloy cast irons; b) nickel-chromium cast irons covering two general types:  4 % Ni 2 % Cr cast irons;  9 % Cr 5 % Ni cast irons; c) high chromium cast irons covering four ranges of chromium content:  11 % < Cr ≤ 14 %;  14 % < Cr ≤ 18 %;  18 % < Cr ≤ 23 %;  23 % < Cr ≤ 30 %. This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast irons which are subject of EN 1564.

BS EN 12513-2011由英国标准学会 GB-BSI 发布于 2011-04-30,并于 2011-04-30 实施。

BS EN 12513-2011 在中国标准分类中归属于: J31 铸造,在国际标准分类中归属于: 77.080.10 铁。

BS EN 12513-2011 发布之时,引用了标准

  • EN ISO 6506-1 金属材料.布氏硬度试验.第1部分:试验方法(ISO 6506-1:2014)*2014-09-01 更新

* 在 BS EN 12513-2011 发布之后有更新,请注意新发布标准的变化。

BS EN 12513-2011的历代版本如下:

BS EN 12513-2011



标准号
BS EN 12513-2011
发布日期
2011年04月30日
实施日期
2011年04月30日
废止日期
中国标准分类号
J31
国际标准分类号
77.080.10
发布单位
GB-BSI
引用标准
EN ISO 6506-1
被代替标准
BS EN 12513-2000
适用范围
This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of:  chemical composition;  hardness. The types of abrasion resistant white cast irons covered by this standard are: a) unalloyed or low alloy cast irons; b) nickel-chromium cast irons covering two general types:  4 % Ni 2 % Cr cast irons;  9 % Cr 5 % Ni cast irons; c) high chromium cast irons covering four ranges of chromium content:  11 % < Cr ≤ 14 %;  14 % < Cr ≤ 18 %;  18 % < Cr ≤ 23 %;  23 % < Cr ≤ 30 %. This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast irons which are subject of EN 1564.




Copyright ©2007-2022 ANTPEDIA, All Rights Reserved