5.1 This test method describes the means of determining the LRV of a tile specimen. Certain building codes require the use of materials rated by LRV. Application of this test method provides the means for rating ceramic tile. LRVs reported for ceramic tile should include reference to the observer and illuminant for which the rating is valid.
5.2 LRV is a property dependent on the overall color of a tile specimen. Control of LRV is achieved through control of color and adherence to color specifications will govern the acceptability of a product with respect to LRV. Therefore, a product cannot be judged as having an unacceptable LRV unless the color of the product is found to be unacceptable.
5.3 Mixtures of several tile products are commonly installed on a surface, requiring a means to calculate LRV for a product mix. The rating obtained for an individual tile product can be used to calculate the LRV for a product mix using the following equation: where:
n = number of products included in the mix p1 to n = the proportion of the surface area taken up by each product, the sum of p1 to pn must equal one LRV1 to n = the LRV for each product used For example, a mixture of two products is used on a surface. Two thirds of the surface area is covered by product A with a LRV of 758201;%, and one third of the surface is covered by product B with an LRV of 608201;% (see Fig. 2). Using the equation, the product mix is found to have an LRV of 708201;%. FIG. 2 Example of a Product Mix Used on a Surface5.4 The test method described herein provides instrumental means as the basis for judging color difference. Magnitude of color difference between pairs of ceramic tile can be determined and expressed in numerical terms.
5.5 Based on interlaboratory investigation,3 color difference ΔE of plain-colored tile, if determined according to this test method, should give excellent reproducibility with a standard deviation of not more than σ8201;=8201;±0.15 units. LRV should also give excellent reproducibility when used for solid colored tile based on the relationship between LRV and either the Y tristimulus or L value. However, LRV reproducibility for multicolored, speckled, or textured surface tile will be dependent upon the degree of variation of the tile specimen, and will require a different measurement procedure to minimize the impact of the variation.
5.6 The test method requires the use of multiple illuminants for the determinati......
边直度、直角度 ASTM C502 翘曲度 ASTM C485 有釉砖抗热震 ASTM C484 耐化学腐蚀 ASTM C650 有釉砖表面耐磨 ASTM C1027 无釉砖耐磨深度 ASTM C1243 吸水率 ASTM C373-88(2006) 小色差 ASTM C609-07 破坏强度 ASTM C648 抗龟裂 ASTM C424 ...
分散有机物反射率测量的标准化在油气勘探中,镜质体反射率被认为是测定热成熟度最可靠的岩石学参数,但是,长期以来在非煤沉积岩样品的实验室间研究难以获得可重复的测量结果。为了解决这个短板,一个由政府、学术界、工业界和咨询公司的技术专家组成的国际委员会编写了ASTM(美国测试与材料协会)标准测试方法D7708 (ASTM, 2014a)以满足除煤以外岩石(尤其是页岩)反射率测量标准化的需求。...
色差仪CR-400/410可以根据客户需要自定义色彩评价公式,来代替通用的色彩测量公式;色差仪CR-400/410加上数据处理器最多可以存储2000个数据。 4、色差仪CR-10标准偏差DE*ab 0.1以内(测量条件:标准白板测量平均值); 色差仪CR-400/410标准偏差ΔE*ab 0.07以内(白色校正后在10秒间隔内测定30次时)。 ...
Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号