本文件规定了电动注塑机用高性能球墨铸铁移动锁模板(以下简称“移动板”)的术语和定义、基本要求、技术要求、试验方法、检验规则、标志、包装、运输和贮存及质量承诺。 本文件适用于电动注塑机锁模机构的高性能球墨铸铁移动模板材料成型和精加工、防腐要求。

High performance ductile iron movable platen for electric injection molding machine

ICS
77.140.80
CCS
C339
发布
2022-12-08
实施
2023-04-04

本文件规定了不锈钢泵体精密铸件(以下简称泵体铸件) 的基本要求、技术要求、性能要求、试验方法、检验规则、标志、 包装、运输和贮存及质量承诺。 本文件适用于熔模铸造工艺生产的用于液态介质输送的不锈钢泵体精密铸件。

Precision casting of stainless steel pump body

ICS
77.140.80
CCS
C339
发布
2022-12-08
实施
2023-03-31

本文件规定了重型履带板铸钢件(以下简称铸件)的牌号、技术要求、试验方法、检验规则,以及标志、贮存、包装和运输等。 本文件适用于冶金、矿山、电力、和机械等行业的大型履带式工程机械履带板铸钢件的制造和验收。其他类型铸造履带件亦可参照执行。

Steel castings for heavy track shoe

ICS
77.140.80
CCS
C339
发布
2022-12-01
实施
2023-03-01

本文件规定了压缩天然气(以下简称CNG)发动机用耐热疲劳铁素体蠕墨铸铁的材料牌号、技术要求、生产方法、试验方法、检验规则与判定、以及标识、质量证明书、包装与贮存、运输和防护。 本文件适用于砂型、壳型铸造方法生产的、使用温度不大于 850 ℃ 的CNG发动机用 耐热疲劳铁素体蠕墨铸铁涡轮壳,其它铸造方法生产的CNG发动机及其它燃料发动机用 耐热疲劳铁素体蠕墨铸铁件,可参照使用。

Thermal fatigue resistant ferritic vermicular graphite iron castings for compressed natural gas engines

ICS
77.140.80
CCS
C339
发布
2022-11-02
实施
2023-02-02

1.1 This specification covers carbon and alloy steel castings for pressure-containing and other applications intended primarily for petroleum and gas pipelines in areas subject to lowambient temperatures. Castings shall be heat treated by normalizing and tempering or liquid quenching and tempering. All classes are weldable under proper conditions. Hardenability of some grades may limit usable section size. 1.2 The values stated in either inch-pound units or SI units are to be regarded separately as standard. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.2.1 Unless the order specifies an “M” designation, the material shall be furnished to inch-pound units. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Steel Castings, Ferritic and Martensitic, for Pressure-Containing and Other Applications, for Low-Temperature Service

ICS
77.140.80
CCS
发布
2022-11-01
实施

1.1 This specification covers castings of ferritic, pearlitic, tempered pearlitic, and tempered martensitic grades of malleable iron used in the products of the automotive and allied industries. Castings shall be heat treated to meet this specification. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Automotive Malleable Iron Castings

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification2 covers centrifugally cast cylinders with an outer layer of white cast iron and the remainder of the material of gray cast iron. These castings are suitable for pressure-containing parts, the design strength of which is based on the gray iron portion of the cylinder. These castings are suitable for service at temperatures up to 450 °F [230 °C]. 1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.3 The following safety hazards caveat pertains only to the test method portion, Section 8, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Centrifugally Cast Dual Metal (Gray and White Cast Iron) Cylinders

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers ductile iron castings for use in pressure-containing paper mill dryer rolls at temperatures up to 450 °F [230 °C]. 1.2 No precise quantitative relationship can be stated between the properties of the iron in various locations of the same casting or between the properties of a casting and those of a test specimen cast from the same iron (see Appendix X1). 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.3.1 Exception—Within the text, the SI units are shown in brackets. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Ductile Iron Castings for Paper Mill Dryer Rolls

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification2 covers ferritic malleable castings for general engineering usage at temperatures from normal ambient to approximately 400 °C [750 °F]. 1.2 No precise quantitative relationship can be stated between the properties of the iron in various locations of the same casting and those of a test specimen cast from the same iron (see Appendix X1). 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Ferritic Malleable Iron Castings

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers austenitic ductile iron castings, which are used primarily for their resistance to heat, corrosion, and wear, and for other special purposes. 1.2 Austenitic ductile iron, also known as austenitic nodular iron or austenitic spheroidal iron, is characterized by having its graphite substantially in a spheroidal form and substantially free of flake graphite. It contains some carbides and sufficient alloy content to produce an austenitic structure. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Austenitic Ductile Iron Castings

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers high-silicon cast iron castings intended for corrosion-resistant service. 1.2 This specification covers three grades as shown in Table 1. Selection of grade depends on the corrosive service to be experienced by the casting. All three grades are suited for application in severe corrosive environments. However, Grade 2 is particularly suited for application in strong chloride environments, and Grade 3 is recommended for impressed current anodes. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.4 The following safety hazards caveat pertains only to the test method portion, Section 9, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Corrosion-Resistant High-Silicon Iron Castings

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers pearlitic malleable iron castings for general engineering usage at temperatures from normal ambient to approximately 750 °F [400 °C]. 1.1.1 For continuous service at temperatures up to 1200 °F [650 °C], design factors should be incorporated to compensate for possible property changes, as demonstrated by Marshall and Sommer2 and by Pearson.3 1.2 Without knowledge of casting geometry and process details, no quantitative relationship can be stated between the properties of the iron in the various locations of a casting and those of a test bar cast from the same iron. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Pearlitic Malleable Iron

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers ductile iron castings for pressure-retaining parts for use at elevated temperatures. Castings of all grades are suitable for use up to 450 °F. For temperatures above 450 °F and up to 650 °F, only Grade 60-40-18 castings are suitable (Note 1). 1.2 Valves, flanges, pipe fittings, pumps, and other piping components are generally manufactured in advance and supplied from stock by the manufacturer, jobber, or dealer. 1.3 For supplemental casting requirements, Specification A834 may be utilized. 1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. NOTE 1—For service other than as specified in this section, reference should be made to Specification A536 for Ductile Iron Castings.2 1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers ductile iron castings suitable for service at temperatures of −40 °F [–40 °C] and above. 1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.3 The following precautionary statement pertains only to the test methods portion, Section 11, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Ferritic Ductile Iron Castings Suitable for Low-Temperature Service

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers ductile iron castings that are subsequently heat treated by an austempering process as defined in 9.1. 1.2 The application of the austempering heat treatment extends the range of properties achievable in ductile iron castings. 1.3 No precise quantitative relationship can be stated between the properties of the iron in various locations of the same casting or between the properties of castings and those of a test specimen cast from the same iron (see Appendix X1). However, austempering heat treatment will tend to diminish any differences in mechanical properties. 1.4 The production of castings, machining (if required), and the austempering heat treatments may be performed by different manufacturers, as covered in Section 13. The purchaser should establish by contract agreement, at the time of ordering, the responsibility of the various parties for meeting the specification requirements. 1.5 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.5.1 Exception—Within the text, the SI units are shown in brackets. 1.6 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Austempered Ductile Iron Castings

ICS
77.140.80
CCS
发布
2022-10-01
实施

1.1 This specification covers statically cast dual metal rolls with the outer layer of the roll body being chilled white iron of different chemical composition than the core and journals of the roll which is gray cast iron. The castings are suitable for pressure-containing parts, the design strength of which is based on the gray iron portion of the cylinder. The castings are suitable for service at temperatures up to 450 °F [232 °C]. 1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard. 1.3 The following safety hazards statement pertains only to the test method portion, Section 9, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Statically Cast Chilled White Iron-Gray Iron Dual Metal Rolls for Pressure Vessel Use

ICS
77.140.80
CCS
发布
2022-10-01
实施

本文件规定了采用铁型覆砂铸造工艺生产的汽车制动鼓铸件的术语和定义、技术要求、试验方法、检验规则、标志和质量证明书以及包装、运输和贮存。

Iron based coated sand brake drum casting

ICS
77.140.80
CCS
C3670
发布
2022-08-30
实施
2022-09-01

本文件规定了汽车用双金属复合制动鼓术语和定义、分类、技术要求、试验方法、检验规则、标志和质量证明书以及包装、运输和贮存。

Bimetal composite brake drum

ICS
77.140.80
CCS
C3670
发布
2022-08-30
实施
2022-09-01

Testing methods for clad steel

ICS
77.140.80
CCS
发布
20220816
实施
20220816

Steel castings-General technical delivery requirements

ICS
77.140.80
CCS
发布
20220816
实施
20220816



Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号