Form: This specification covers a cobalt base alloy in the form of powder@ wire@ strip@ foil@ and rod and a viscous mixture of the powder in a suitable liquid plastic binder. Application: Primarily for joining cobalt base alloys where corrosion and oxidation resistant joints with good strength at high temperature are required. Flow well in dry@ reducing or neutral atmospheres and in vacuum.