02016-2003

Fracture toughness (K sub Ic) values of some cast irons


说明:

  • 此图仅显示与当前标准最近的5级引用;
  • 鼠标放置在图上可以看到标题编号;
  • 此图可以通过鼠标滚轮放大或者缩小;
  • 表示标准的节点,可以拖动;
  • 绿色表示标准:02016-2003 , 绿色、红色表示本平台存在此标准,您可以下载或者购买,灰色表示平台不存在此标准;
  • 箭头终点方向的标准引用了起点方向的标准。

 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 02016-2003 前三页,或者稍后再访问。

点击下载后,生成下载文件时间比较长,请耐心等待......

 



标准号
02016-2003
发布日期
2003年03月01日
实施日期
2004年05月14日
废止日期
中国标准分类号
/
国际标准分类号
/
发布单位
ESDU - Engineering Sciences Data Unit
引用标准
209
适用范围
Data Item No. 02016 provides both static and dynamic fracture toughness data for over 150 specifications of cast iron in the grey@ chilled@ white@ malleable@ ductile and compacted graphite forms. Also included are detailed descriptions of the general nature of these irons@ and their respective fracture characteristics. Additionally@ the factors likely to influence a measured fracture toughness value for a given material are considered@ as are the peculiarities experienced with fracture toughness testing of cast iron. The fracture toughness data appearing in the Item fall within the temperature ranges of interest for practical applications@ with the full brittle-to-ductile transition spectrum being considered for a number of ductile irons. The applicability of the Barsom Temperature Shift to static fracture toughness values for ductile iron is also investigated. The Item contains an in-depth statistical analysis@ offering the user two methods for obtaining a design allowable fracture toughness value with a prescribed level of confidence. The first method is the result of studies of the correlation between the fracture toughness of various forms of cast iron and other parameters: hardness (white and grey cast irons)@ tensile strength (grey cast iron)@ and temperature (ductile iron). The second method is based on the provision of mean fracture toughness values for each type of material@ from which design allowable values can be calculated. A worked example illustrates the implementation of these techniques@ and guidance is given on the applicability of each method. Standard requirements for cast iron compositions and mechanical properties are provided@ and discrepancies in cast iron fracture toughness measurements obtained through the use of different variants of a standard test procedure are considered.




Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号