77017 B-1979

Endurance of titanium alloy lugs (Ti-6Al-4V@ annealed and Ti-4Al-4Mo-2Sn-0.5Si).


 

 

非常抱歉,我们暂时无法提供预览,您可以试试: 免费下载 77017 B-1979 前三页,或者稍后再访问。

如果您需要购买此标准的全文,请联系:

点击下载后,生成下载文件时间比较长,请耐心等待......

 

标准号
77017 B-1979
发布日期
1979年10月01日
实施日期
2004年05月14日
废止日期
中国标准分类号
/
国际标准分类号
/
发布单位
ESDU - Engineering Sciences Data Unit
引用标准
10
适用范围
ESDU 77017 gives data for constant-amplitude fatigue tests drawn from mainly unpublished sources. The data are plotted as an alternating stress parameter (involving the stress concentration and the material tensile strength) against endurance. For Ti-6Al-4V three graphs are given@ one for lugs without bushes which shows the effect of mean stress@ one for lugs without bushes where the material around the hole has been cold-worked@ and one for lugs with close-fitted steel bushes. For Ti-4Al-4Mo-2Sn-0.5Si@ a graph gives data for lugs with fitted copper alloy bushes. Geometrical details of the test specimens are tabulated.




Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号