ZH
RU
ES
toughness of resin
toughness of resin, Total:497 items.
In the international standard classification, toughness of resin involves: Construction materials, Paint ingredients, Plastics, Paints and varnishes, Aircraft and space vehicles in general, Spices and condiments. Food additives, Reinforced plastics, Non-textile floor coverings, Materials for the reinforcement of composites, Organic chemicals, Products of the chemical industry, Interior finishing, Photography, Mechanical testing, Inks. Printing inks, Electrical wires and cables, Paper products, Graphic technology, Paper and board, Raw materials for rubber and plastics, Insulating materials, Pipeline components and pipelines, Protection against fire, Electrical accessories, Rubber and plastics products, Elements of buildings, Materials for aerospace construction, Animal feeding stuffs, Waxes, bituminous materials and other petroleum products, Extraction and processing of petroleum and natural gas, Analytical chemistry, Lifting equipment, Iron and steel products, Ferrous metals, Fasteners, Wood-based panels, Protection of and in buildings, Dentistry, Wood technology processes, Surface treatment and coating, Materials and components for railway engineering, Agricultural machines, implements and equipment, Kitchen equipment, Rotating machinery, Road vehicles in general, Ground service and maintenance equipment, Vocabularies, Pharmaceutics, Components for electrical equipment, Storage equipment.
IPC - Association Connecting Electronics Industries, toughness of resin
American Society for Testing and Materials (ASTM), toughness of resin
- ASTM D2453-99 Standard Test Method for Shrinkage and Tenacity of Oil- and Resin-Base Caulking Compounds
- ASTM D2453-15(2020)e1 Test method for shrinkage and toughness of oil-based and resin-based caulking compounds
- ASTM D2453-03(2009) Standard Test Method for Shrinkage and Tenacity of Oil- and Resin-Base Caulking Compounds
- ASTM D2453-03 Standard Test Method for Shrinkage and Tenacity of Oil- and Resin-Base Caulking Compounds
- ASTM D2453-15 Standard Test Method for Shrinkage and Tenacity of Oil- and Resin-Base Caulking Compounds
- ASTM D6887-03(2013) Standard Test Method for Testing Alkyd Compatibility with Resin or Resin Solutions
- ASTM D3531/D3531M-11 Standard Test Method for Resin Flow of Carbon Fiber-Epoxy Prepreg
- ASTM D6887-03e1 Standard Test Method for Testing Alkyd Compatibility with Resin or Resin Solutions
- ASTM D6887-03 Standard Test Method for Testing Alkyd Compatibility with Resin or Resin Solutions
- ASTM D3531-99(2004) Standard Test Method for Resin Flow of Carbon Fiber-Epoxy Prepreg
- ASTM D3531-99 Standard Test Method for Resin Flow of Carbon Fiber-Epoxy Prepreg
- ASTM D6887-03(2008) Standard Test Method for Testing Alkyd Compatibility with Resin or Resin Solutions
- ASTM F2136-01e1 Standard Test Method for Notched, Constant Ligament-Stress (NCLS) Test to Determine Slow-Crack-Growth Resistance of HDPE Resins or HDPE Corrugated Pipe
- ASTM F2136-08 Standard Test Method for Notched, Constant Ligament-Stress (NCLS) Test to Determine Slow-Crack-Growth Resistance of HDPE Resins or HDPE Corrugated Pipe
- ASTM F2136-18 Standard Test Method for Notched, Constant Ligament-Stress (NCLS) Test to Determine Slow-Crack-Growth Resistance of HDPE Resins or HDPE Corrugated Pipe
- ASTM D6887-03(2020) Standard Test Method for Testing Alkyd Compatibility with Resin or Resin Solutions
- ASTM D5813-95 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Pipe
- ASTM D4142-89(2001) Standard Guide for Testing Epoxy Resins
- ASTM D4142-89(1996)e1 Standard Guide for Testing Epoxy Resins
- ASTM D3643-98(2004) Standard Test Method for Acid Number of Certain Alkali-Soluble Resins
- ASTM D3643-98 Standard Test Method for Acid Number of Certain Alkali-Soluble Resins
- ASTM D709-16 Standard Specification for Laminated Thermosetting Materials
- ASTM D5801-95(2006) Standard Test Method for Toughness and Tenacity of Bituminous Materials
- ASTM D5801-17 Standard Test Method for Toughness and Tenacity of Asphalt Materials
- ASTM D3642-98 Standard Test Method for Softening Point of Certain Alkali-Soluble Resins
- ASTM D6302-98(2009) Standard Practice for Evaluating the Kinetic Behavior of Ion Exchange Resins
- ASTM D5958-99(2020) Standard Practices for Preparation of Oil-Based Ink Resin Solutions
- ASTM D3643-15 Standard Test Method for Acid Number of Certain Alkali-Soluble Resins
- ASTM D4640-86(1996) Standard Test Method for Determining Stroke Cure Time of Thermosetting Phenol-Formaldehyde Resins
- ASTM D3643-15(2022) Standard Test Method for Acid Number of Certain Alkali-Soluble Resins
- ASTM D1763-94 Standard Specification for Epoxy Resins
- ASTM D1763-00 Standard Specification for Epoxy Resins
- ASTM D1763-00(2005) Standard Specification for Epoxy Resins
- ASTM D1763-00(2013) Standard Specification for Epoxy Resins
- ASTM D5801-12 Standard Test Method for Toughness and Tenacity of Bituminous Materials
- ASTM D1259-06(2012) Standard Test Methods for Nonvolatile Content of Resin Solutions
- ASTM D3837-95(2007) Standard Practice for Preparing a Solution of Alkali-Soluble Resins
- ASTM D3837-95(2002) Standard Practice for Preparing a Solution of Alkali-Soluble Resins
- ASTM D3837-95 Standard Practice for Preparing a Solution of Alkali-Soluble Resins
- ASTM D3642-98(2010) Standard Test Method for Softening Point of Certain Alkali-Soluble Resins
- ASTM D3642-98(2004) Standard Test Method for Softening Point of Certain Alkali-Soluble Resins
- ASTM D3837-95(2012) Standard Practice for Preparing a Solution of Alkalindash;Soluble Resins
- ASTM D3642-13(2021) Standard Test Method for Softening Point of Certain Alkali-Soluble Resins
- ASTM D3642-13 Standard Test Method for Softening Point of Certain Alkali-Soluble Resins
- ASTM D6440-10(2018) Standard Terminology Relating to Hydrocarbon Resins
- ASTM E1396-90(1997)e1 Standard Test Method for Sensory Evaluation of Oleoresin Capsicum
- ASTM E1396-90(2017) Standard Test Method for Sensory Evaluation of Oleoresin Capsicum
SAE - SAE International, toughness of resin
Professional Standard - Forestry, toughness of resin
ES-AENOR, toughness of resin
AENOR, toughness of resin
- UNE 48114:1960 QUALITATIVE TESTS OF RESIN
- UNE 48115:1961 QUALITATIVE TESTS FOR PHENOLIC RESINS
- UNE-EN ISO 11402:2006 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004)
- UNE-EN ISO 9771:1997 PLASTICS. PHENOLIC RESINS. DETERMINATION OF THE PSEUDO-ADIABATIC TEMPERATURE RISE OF LIQUID RESOLS WHEN CURED UNDER ACID CONDITIONS (ISO 9771:1995).
- UNE-EN ISO 3673-2:2013 Plastics - Epoxy resins - Part 2: Preparation of test specimens and determination of properties of crosslinked epoxy resins (ISO 3673-2:2012)
- UNE-EN ISO 9944:1996 PLASTICS. PHENOLIC RESINS. DETERMINATION OF ELECTRICAL CONDUCTIVITY OF RESIN EXTRACTS. (ISO 9944:1990).
- UNE-EN 60893-3-6:2004/A1:2010 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes -- Part 3-6: Specifications for individual materials - Requirements for rigid laminated sheets based on silicone resins
- UNE-EN 60893-3-4:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes -- Part 3-4: Specifications for individual materials - Requirements for rigid laminated sheets based on phenolic resins
- UNE-EN 60893-3-6:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes -- Part 3-6: Specifications for individual materials - Requirements for rigid laminated sheets based on silicone resins
- UNE-EN 60893-3-2:2004/A1:2011 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-2: Specifications for individual materials - Requirements for rigid laminated sheets based on epoxy resins
- UNE-EN 60893-3-4:2004/A1:2013 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-4: Specifications for individual materials - Requirements for rigid laminated sheets based on phenolic resins
- UNE-EN 60455-3-1:2004 Resin based reactive compounds used for electrical insulation -- Part 3: Specifications for individual materials - Sheet 1: Unfilled epoxy resinous compounds
TR-TSE, toughness of resin
Japanese Industrial Standards Committee (JISC), toughness of resin
RU-GOST R, toughness of resin
- GOST 29326-2015 Plastics. Phenolic resins. Determination of reactivity of resols under acid conditions
- GOST 26194-1984 Resins for paint and varnish. Methods for determination of hydroxyl number of alkyd and polyester resins
- GOST 29327-1992 Plastics. Liquid phenolic resins. Determination of water mixibility
- GOST R 50492-1993 Plastics. Liquid epoxide resins. Determination of tendency to cristallize
- GOST R 52078-2003 Wood particle boards, laminated with paper impregnated with thermosetting resins
- GOST 32289-2013 Wood particleboards, laminated with paper impregnated with thermosetting resins
- GOST 22304-2015 Unsaturated polyester resins. Methods for determination of acid value
- GOST R 57687-2017 Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry
PL-PKN, toughness of resin
- PN C89085-24-1988 Epoxy resins Methóds of testing Determination of properties of cured resins
- PN C89082-17-1988 Unsaturated polyester resins Methods of testing Determination of properties of cured resins
- PN C89044-1975 Plastics Phenolic resins Determination of free phenols
- PN E29080-1988 Insulating materials Laminated sheets based on thermosetting resins
- PN C89272-1991 Phenolic resins. Alkoholic solutions of the resol resins
- PN C89085-10-1986 Epoxy resins Methods of testing Determination of volatile and nonvolatile matter
- PN C89085-11-1987 Epoxy resins Methods of testing Determination of durability in elevated temperatur?
- PN C89085-20-1988 Epoxy rcsins Mcthods ol testing Determination ol pot time of resin alter mixing with hardener
Group Standards of the People's Republic of China, toughness of resin
U.S. Military Regulations and Norms, toughness of resin
- ARMY MIL-R-47004 VALID NOTICE 1-1990 RESIN, EPOXY BASE, THIXOTROPIC
- ARMY MIL-R-47004-1974 RESIN, EPOXY BASE, THIXOTROPIC
- ARMY UFGS-32 12 18-2008 RESIN MODIFIED PAVEMENT SURFACING MATERIAL
- ARMY A-A-56031 VALID NOTICE 2-2009 Adhesive, Epoxy, Modified, Flexible, Two Component
- ARMY MIL-DTL-53030 C-2010 PRIMER COATING, EPOXY, WATER BASED, LEAD AND CHROMATE FREE
- ARMY MIL-P-46067 B NOTICE 3-2000 PLASTIC EMBEDDING COMPOUND, EPOXY RESIN SYSTEM
- ARMY MIL-P-46067 B REINST NOTICE 2-2000 PLASTIC EMBEDDING COMPOUND, EPOXY RESIN SYSTEM
- ARMY MIL-P-46067 B-1977 PLASTIC EMBEDDING COMPOUND, EPOXY RESIN SYSTEM
- ARMY MIL-E-52835 A (2)-1980 ENAMEL, MODIFIED ALKYD, CAMOUFLAGE, LUSTERLESS
- ARMY MIL-E-52835 A-1976 ENAMEL, MODIFIED ALKYD, CAMOUFLAGE, LUSTERLESS
- ARMY MIL-DTL-53030 D-2011 PRIMER COATING, EPOXY, WATER BASED, LEAD AND CHROMATE FREE
RO-ASRO, toughness of resin
CZ-CSN, toughness of resin
SE-SIS, toughness of resin
Association Francaise de Normalisation, toughness of resin
- NF EN ISO 11402:2005 Résines phénoliques, aminiques et de condensation - Dosage du formaldéhyde libre
- NF T51-405*NF EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content.
- NF P62-301:1996 Resilient floor coverings. Polyvinyl chloride floor coverings on jute backing or on polyester felt backing or on polyester felt with polyvinyl chloride backing. Specification.
- NF EN ISO 9771:1997 Plastiques - Résines phénoliques - Détermination de l'élévation de température pseudoadiabatique des résols liquides thermodurcis en conditions acides.
- NF T77-101:1985 Basic silicones for industrial use. Determination of density.
- NF EN ISO 3673-2:2012 Plastiques - Résines époxydes - Partie 2 : préparation des éprouvettes et détermination des propriétés des résines époxydes réticulées
- NF T51-520-2*NF EN ISO 3673-2:2012 Plastics - Epoxy resins - Part 2 : preparation of test specimens and determination of properties of crosslinked epoxy resins.
- NF F05-393:1995 PLASTICS. PHENOLIC RESINS. DETERMINATION OF ELECTRICAL CONDUCTIVITY OF RESIN EXTRACTS. (EUROPEAN STANDARD EN ISO 9944).
- NF EN ISO 9944:1995 Plastiques - Résines phénoliques - Détermination de la conductivité électrique des extraits de résine.
- NF T51-527:1985 Plastics. Epoxies. Determination of properties.
- NF T77-111:1988 Basic silicones for industrial use. Determination of flash points.
- NF T51-441*NF EN ISO 9771:1997 Plastics. Phenolic resins. Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions.
- NF T51-516:1985 Plastics. Unsaturated polyester resins. Determination of properties.
- NF EN ISO 8989:1998 Plastiques - Résines phénoliques liquides - Détermination de la tolérance à l'eau.
- NF T25-101*NF EN ISO 10618:2005 Carbon fibre - Determination of tensile properties of resin-impregnated yarn.
- NF ISO 15034:2001 Composites - Préimprégnés - Détermination de l'écoulement de résine
- NF A05-202:1977 Application of separations on ion-exchange resines. Resin types, column making and utilisation.
- NF EN ISO 4615:1999 Plastiques - Résines de polyesters non saturés et époxydes - Détermination de la teneur totale en chlore.
- NF C26-163-8*NF EN IEC 60455-3-8:2021 Resin based reactive compounds used for electrical insulation - Part 3-8 : specifications for individual materials - Resins for cable accessories
- NF EN ISO 10618:2005 Fibres de carbone - Détermination des propriétés en traction sur fils imprégnés de résine
- NF A49-708-1*NF EN 10289:2002 Steel tubes and fittings for onshore and offshore pipelines - External liquid applied epoxy and epoxy-modified coatings
- NF F19-478:1989 Rolling stock. Thermo setting powder paints made of epoxy resins.
- NF T51-423*NF EN ISO 8989:1998 Plastics. Liquid phenolic resins. Determination of water miscibility.
- NF EN IEC 60455-3-8:2021 Composés réactifs à base de résines utilisés comme isolants électriques - Partie 3-8 : spécifications pour matériaux particuliers - Résines pour accessoires de câble
- NF T57-160-3:1994 TEXTILE-GLASS-REINFORCED PLASTICS. DETERMINATION OF MECHANICAL PROPERTIES ON RODS MADE OF ROVING-REINFORCED RESIN. PART 3 : DETERMINATION OF COMPRESSIVE STRENGTH.
- NF T57-160-2:1994 TEXTILE-GLASS-REINFORCED PLASTICS. DETERMINATION OF MECHANICAL PROPERTIES ON RODS MADE OF ROVING-REINFORCED RESIN. PART 2 : DETERMINATION OF FLEXURAL STRENGTH.
- NF C26-183-6/A2*NF EN IEC 60893-3-6/A2:2018 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-6 : specifications for individual materials - Requirements for rigid laminated sheets based on silicone resins
- NF S91-211-2:2010 Dentistry - Water-based cements - Part 2 : resin-modified cements.
- NF T57-160-1:1994 TEXTILE-GLASS-REINFORCED PLASTICS. DETERMINATION OF MECHANICAL PROPERTIES ON RODS MADE OF ROVING-REINFORCED RESIN. PART 1 : GENERAL CONSIDERATIONS AND PREPARATION OF RODS.
- NF EN 10289:2002 Tubes et raccords en acier pour canalisations enterrées et immergées - Revêtements externes en résine époxyde ou époxyde modifiée appliquée à l'état liquide
- NF T51-501*NF EN ISO 3521:1999 Plastics. Unsaturated polyester and epoxy resins. Determination of overall volume shrinkage.
British Standards Institution (BSI), toughness of resin
- BS ISO 21318:2007 Plastics - Epoxy resins - Determination of electrical conductivity of aqueous resin extracts
- BS EN ISO 3673-2:2012 Plastics. Epoxy resins. Preparation of test specimens and determination of properties of crosslinked epoxy resins
- BS EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content
- BS ISO 4216:2021 Thermosetting resin and UV curable resin. Determination of shrinkage by continuous measurement method
- BS EN ISO 9944:1995 Plastics. Phenolic resins. Determination of electrical conductivity of resin extracts
- BS EN IEC 60455-3-8:2021 Resin based reactive compounds used for electrical insulation. Specifications for individual materials. Resins for cable accessories
- BS EN 60455-3-2:2003 Resin based reactive compounds used for electrical insulation - Specifications for individual materials - Quartz filled epoxy resinous compounds - Sheet 2: Quartz filled epoxy resinous compounds
- BS ISO 15034:2000 Composites. Prepregs. Determination of resin flow
- BS EN ISO 8989:1998 Plastics. Liquid phenolic resins. Determination of water miscibility
- BS EN ISO 10618:2004 Carbon fibre - Determination of tensile properties of resin-impregnated yarn
- BS EN ISO 9771:1997 Plastics. Phenolic resins. Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions
- BS EN 60455-3-5:2006 Resin based reactive compounds used for electrical insulation - Specifications for individual materials - Unsaturated polyester based impregnating resins
- 20/30412517 DC BS ISO 4216. Thermosetting resin and UV curable resin. Determination of shrinkage by continuous measurement method
- BS EN 60455-3-5:2002 Resin based reactive compounds used for electrical insulation - Specifications for individual materials - Unsaturated polyester based impregnating resins - Sheet 5: Unsaturated polyester based impregnating resins
- BS EN 60455-3-1:2003 Resin based reactive compounds used for electrical insulation - Specifications for individual materials - Unfilled epoxy resinous compounds - Sheet 1: Unfilled epoxy resinous compounds
- BS EN ISO 10618:2000 Carbon fibre - Determination of tensile properties of resin-impregnated yarns
- BS EN ISO 8130-8:1995 Coating powders. Assessment of the storage stability of thermosetting powders
- BS 7332:1990 Specification for decorative continuous laminates (DCL) based on thermosetting resins
- BS EN ISO 8130-8:2010 Coating powders. Assessment of the storage stability of thermosetting powders
- BS EN 60455-3-8:2013 Resin based reactive compounds used for electrical insulation. Specifications for individual materials. Sheet 8: Resins for cable accessories
- BS EN IEC 60893-3-6:2004+A2:2018 Insulating materials. Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Specifications for individual materials. Requirements for rigid laminated sheets based on silicone resins
Indonesia Standards, toughness of resin
工业和信息化部, toughness of resin
Society of Automotive Engineers (SAE), toughness of resin
- SAE ARP5144-2011 Heat Application for Thermosetting Resin Curing
- SAE AMS3727A-1993 RESIN, EPOXY, MATRIX, THERMOSETTING Moderate Temperature Resistant, Unfilled
- SAE AMS3727-1988 RESIN, EPOXY, MATRIX, THERMOSETTING Moderate Temperature Resistant, Unfilled
- SAE AMS3370A-1988 Silicone Resin, Elastomeric, Transparent Room Temperature Cure
- SAE AMS3368A-1988 Silicone Resin, Elastomeric, Transparent Elevated Temperature Cure
- SAE AMS3368B-2012 Silicone Resin, Elastomeric, Transparent, Elevated Temperature Cure
- SAE AMS3370B-2012 Silicone Resin, Elastomeric, Transparent, Room Temperature Cure
- SAE AMS3681C-2005 Adhesive, Electrically Conductive Silver-Filled Epoxy Resin
- SAE AMS3371-1969 Silicone Resin, Elastomeric, Opaque, Room Temperature Cure
- SAE AMS3137C-1994 RESIN, CONFORMAL COATING, URETHANE ELASTOMER
- SAE AMS3137D-1994 Resin, Conformal Coating, Urethane Elastomer
- SAE AMS3137B-2011 RESIN, CONFORMAL COATING, URETHANE ELASTOMER
- SAE AMS3726C-1998 Shims, Filled Resin Compound
- SAE AMS3368-1968 SILICONE RESIN, ELASTOMERIC, TRANSPARENT ELEVATED TEMPERATURE CURE
- SAE AMS3704-1993 ADHESIVE, CONTACT Chloroprene, Resin Modified
- SAE AMS3750-1994 POTTING COMPOUND, EPOXY, FLEXIBLE Durometer 75 - 85
- SAE AMS3750A-1994 Potting Compound, Epoxy, Flexible Durometer 75-85
- SAE AMS3372A-1988 Silicone Resin, Elastomeric High Tear Strength Elevated Temperature Cure
- SAE AMS3372B-2012 Silicone Resin, Elastomeric, High Tear Strength, Elevated Temperature Cure
- SAE AMS7267G-2001 Rings, Sealing, Silicone (VSI) Rubber Heat-Resistant, Low Compression Set 70 - 80
- SAE AMS3897-1988 Cloth, Carbon Fiber, Resin Impregnated
- SAE ARP5144-2000 Heat Application for Thermosetting Resin Curing
- SAE AMS3726E-2011 Shims, Filled Resin Compound
- SAE AMS3370A-2001 Silicone Resin, Elastomeric, Transparent Room Temperature Cure
- SAE AMS3370-1968 SILICONE RESIN, ELASTOMERIC, TRANSPARENT ROOM TEMPERATURE CURE
- SAE AMS3368A-2001 Silicone Resin, Elastomeric, Transparent Elevated Temperature Cure
- SAE AMS3571-1976 POLYURETHANE CASTING RESIN, FLEXIBLE, SOLID Polyether-Type
Canadian General Standards Board (CGSB), toughness of resin
- CGSB 1-GP-71 METH 75.2-1982 Methods of Testing Paints and Pigments Detection of Resins Qualitative Test for Phenol-Formaldehyde Resins
- CGSB 1-GP-71 METH 82.1-1982 Methodes D'Essai Des Peintures Et Pigments Analyse De La Resine Vinylique Separation Et Identification De La Resine Vinylique (Analyse Qualitative)
Korean Agency for Technology and Standards (KATS), toughness of resin
International Organization for Standardization (ISO), toughness of resin
- ISO 11402:2004 Phenolic, amino and condensation resins - Determination of free-formaldehyde content
- ISO 9944:1990 Plastics; phenolic resins; determination of electrical conductivity of resin extracts
- ISO 9771:1995 Plastics - Phenolic resins - Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions
- ISO 4895:2014 Plastics - Liquid epoxy resins - Determination of tendency to crystallize
- ISO 4216:2021 Thermosetting resin and UV curable resin — Determination of shrinkage by continuous measurement method
- ISO/TR 23602:2005 Toughness of chain steels
- ISO 9371:1990 Plastics; phenolic resins in the liquid state or in solution; determination of viscosity
- ISO 8989:1988 Plastics; liquid phenolic resins; determination of water miscibility
- ISO 10618:1999 Carbon fibre - Determination of tensile properties of resin-impregnated yarn
- ISO 10618:2004 Carbon fibre - Determination of tensile properties of resin-impregnated yarn
- ISO 9944:1990/cor 1:1997 Plastics - Phenolic resins - Determination of electrical conductivity of resin extracts; Technical Corrigendum 1
- ISO 4895:1987 Plastics; Liquid epoxide resins; Determination of tendency to crystallize
- ISO 1642:1975 Title missing - Legacy paper document
- ISO 1642:1987 Plastics; Industrial laminated sheets based on thermosetting resins; Specification
- ISO 1642:1979 Plastics — Industrial laminated sheets based on thermosetting resins — Specification
- ISO 9917-2:2017 Dentistry — Water-based cements — Part 2: Resin-modified cements
- ISO 14656:1999 Epoxy powder and sealing material for the coating of steel for the reinforcement of concrete
Danish Standards Foundation, toughness of resin
- DS/EN ISO 11402/AC:2006 Phenolic, amino and condensation resins - Determination of free-formaldehyde content
- DS/EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content
- DS/EN ISO 3673-2:2012 Plastics - Epoxy resins - Part 2: Preparation of test specimens and determination of properties of crosslinked epoxy resins
- DS/EN ISO 9944:1996 Plastics - Phenolic resins - Determination of electrical conductivity of resin extracts
- DS/EN ISO 10618:2004 Carbon fibre - Determination of tensile properties of resin-impregnated yarn
- DS/EN ISO 8989:1999 Plastics - Liquid phenolic resins - Determination af water miscibility
- DS/EN ISO 9771:1997 Plastics - Phenolic resins - Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions
- DS/EN IEC 60455-3-8:2021 Resin based reactive compounds used for electrical insulation – Part 3-8: Specifications for individual materials – Resins for cable accessories
- DS/EN 60455-3-8:2013 Resin based reactive compounds used for electrical insulation - Part 3: Specifications for individual materials - Sheet 8: Resins for cable accessories
- DS/EN 60893-3-2/A1:2011 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-2: Specifications for individual materials - Requirements for rigid laminated sheets based on epoxy resins
- DS/EN 60893-3-2:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-2: Specifications for individual materials - Requirements for rigid laminated sheets based on epoxy resins
- DS/EN 60893-3-4:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-4: Specifications for individual materials - Requirements for rigid laminated sheets based on phenolic resins
- DS/EN 60893-3-5/A1:2009 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-5: Specifications for individual materials - Requirements for rigid laminated sheets based on polyester resins
- DS/EN 60893-3-5:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-5: Specifications for individual materials - Requirements for rigid laminated sheets based on polyester resins
- DS/EN 60893-3-6/A1:2010 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-6: Specifications for individual materials - Requirements for rigid laminated sheets based on silicone resins
- DS/EN 60893-3-6:2004 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-6: Specifications for individual materials - Requirements for rigid laminated sheets based on silicone resins
- DS/EN 60893-3-4/A1:2013 Insulating materials - Industrial rigid laminated sheets based on thermosetting resins for electrical purposes - Part 3-4: Specifications for individual materials - Requirements for rigid laminated sheets based on phenolic resins
German Institute for Standardization, toughness of resin
- DIN EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004); German version of EN ISO 11402:2005
- DIN EN ISO 11402 Berichtigung 1:2006 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004); German version EN ISO 11402:2005, Corrigenda to DIN EN ISO 11402:2005-09; German version EN ISO 11402:2005/AC:2006
- DIN EN ISO 11402:2005-09 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004); German version of EN ISO 11402:2005
- DIN EN ISO 11402 Berichtigung 1:2006-11 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004); German version EN ISO 11402:2005, Corrigenda to DIN EN ISO 11402:2005-09; German version EN ISO 11402:2005/AC:2006
- DIN 16945:1989 Testing of resins, hardeners and accelerators, and catalyzed resins
- DIN ISO 9944:1992 Plastics; phenolic resins; determination of electrical conductivity of resin extracts; identical with ISO 9944:1990
- DIN EN ISO 8989:1998-10 Plastics - Phenolic resins - Determination of water miscibility (ISO 8989:1995); German version EN ISO 8989:1998
- DIN EN ISO 3673-2:2012-10 Plastics - Epoxy resins - Part 2: Preparation of test specimens and determination of properties of crosslinked epoxy resins (ISO 3673-2:2012); German version EN ISO 3673-2:2012
- DIN 16945:1989-03 Testing of resins, hardeners and accelerators, and catalyzed resins
- DIN 54407:2015 Testing of ion exchange resins - Determination of bead size distribution
- DIN 54407:2003 Testing of ion exchange resins - Determination of bead size distribution
- DIN 18556:1985 Testing of coating material for synthetic resin plasters and of synthetic resin plasters
- DIN EN ISO 10618:2004 Carbon fibre - Determination of tensile properties of resin-impregnated yarn (ISO 10618:2004); German version EN ISO 10618:2004
- DIN EN ISO 10618:2004-11 Carbon fibre - Determination of tensile properties of resin-impregnated yarn (ISO 10618:2004); German version EN ISO 10618:2004
- DIN EN ISO 9771:1997 Plastics - Phenolic resins - Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions (ISO 9771:1995); German version EN ISO 9771:1997
- DIN EN ISO 9771:1997-05 Plastics - Phenolic resins - Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions (ISO 9771:1995); German version EN ISO 9771:1997
- DIN 51290-2:1991 Testing of polymer concretes (reaction resin concretes) for mechanical engineering purposes; testing of binders, fillers and reaction resin compounds
- DIN ISO 9944:1992-06 Plastics; phenolic resins; determination of electrical conductivity of resin extracts; identical with ISO 9944:1990
- DIN 55954:1990 Binders for paints and varnishes; compatibility (miscibility behaviour) test for resins
未注明发布机构, toughness of resin
- BS EN ISO 11402:2005(2006) Phenolic, amino and condensation resins — Determination of free - formaldehyde content
- BS EN ISO 9944:1995(1999) Plastics — Phenolic resins — Determination of electrical conductivity ofresin extracts
- BS EN 60893-3-4:2004+A1:2012(2014) Insulating materials — Industrial rigid laminated sheets based on thermosetting resins for electrical purposes — Part 3 - 4 : Specifications for individual materials — Requirements for rigid laminated sheets based on phenolic resins
Professional Standard - Chemical Industry, toughness of resin
HU-MSZT, toughness of resin
Taiwan Provincial Standard of the People's Republic of China, toughness of resin
- CNS 11366-1985 Decorative Laminated Sheet Based on Thermosetting Resins
- CNS 2182-1997 Oleo-resinous enamelled round copper winding wires
- CNS 3707-1973 Phenol and Formaldehyde Content in Extract of Phenolic Resin or Other Thermosetting Resins Dinner Wares
- CNS 11367-1985 Method of Test for Decorative Laminated Sheet Based on Thermosetting Resins
- CNS 9352-1982 Bushes for Plain Bearings Made From Dura Plastics
- CNS 11557-1986 Acrylic Denture Base Resin
- CNS 9977-1983 Enamelled Resistance Wires and Oleo-Resinous Enamelled Silk Covered Resistance Wires
United States Navy, toughness of resin
- NAVY QPL-85582-2013 Primer Coatings: Epoxy, Waterborne
- NAVY QPL-85582-QPD-2011 Primer Coatings: Epoxy, Waterborne
- NAVY QPL-631-QPD-2012 Insulation, Electrical, Synthetic-Resin Composition, Nonrigid
- NAVY QPL-631-2012 Insulation, Electrical, Synthetic - Resin Composition, Nonrigid
- NAVY QPL-631-73-2005 INSULATION, ELECTRICAL, SYNTHETIC RESIN COMPOSITION, NONRIGID
- NAVY MIL-PRF-85582 E-2012 PRIMER COATINGS: EPOXY, WATERBORNE
- NAVY MIL-I-631 D (6)-1987 INSULATION, ELECTRICAL, SYNTHETIC-RESIN COMPOSITION, NONRIGID
- NAVY MIL-I-631 D-1961 INSULATION, ELECTRICAL, SYNTHETIC-RESIN COMPOSITION, NONRIGID
- NAVY A-A-50605-1993 EXPANSION JOINT, TFE FLUOROCARBON RESIN, CORRUGATED WITH DUCTILE IRON FLANGES
- NAVY QPL-631-73 NOTICE 1-2008 Insulation, Electrical, Synthetic-Resin Composition, Nonrigid
- NAVY QPL-631-QPD-2010 Insulation, Electrical, Synthetic - Resin Composition, Nonrigid
- NAVY QPL-631-QPD-2011 Insulation, Electrical, Synthetic - Resin Composition, Nonrigid
- NAVY QPL-631-2011 Insulation, Electrical, Synthetic - Resin Composition, Nonrigid
GM Europe, toughness of resin
US-FCR, toughness of resin
工业和信息化部/国家能源局, toughness of resin
- JB/T 13574-2018 Resin-based active compound epoxy drip impregnating resin for electrical insulation
- JB/T 13575-2018 Resin-based reactive compound epoxy continuous impregnated resin for electrical insulation
European Committee for Standardization (CEN), toughness of resin
- EN ISO 11402:1998 Plastics - Condensation Resins - Determination of Free Formaldehyde ISO 11402:1993
- EN 650:1996 Resilient Floor Coverings - Polyvinyl Chloride Floor Coverings on Jute Backing or on Polyester Felt Backing or on Polyester Felt with Polyvinyl Chloride Backing - Specification
- EN ISO 11402:2005/AC:2006 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004)
- EN 1796:2013 Plastics piping systems for water supply with or without pressure - Glass-reinforced thermosetting plastics (GRP) based on unsaturated polyester resin (UP)
- EN ISO 9371:1995 Plastics - Phenolic Resins in the Liquid State or in Solution - Determination of Viscosity (ISO 9371 : 1990)
- EN ISO 9944:1995 Plastics - Phenolic Resins - Determination of Electrical Conductivity of Resin Extracts (ISO 9944 : 1990)
- EN ISO 10618:1999 Carbon Fibre - Determination of Tensile Properties of Resin-Impregnated Yarns ISO 10618: 1999
- EN ISO 8989:1995 Plastics - Liquid Phenolic Resins - Determination of Water Miscibility (ISO 8989 : 1988)
- EN 10289:2002 Steel tubes and fittings for onshore and offshore pipelines - External liquid applied epoxy and epoxy-modified coatings
- EN ISO 4895:2014 Plastics - Liquid epoxy resins - Determination of tendency to crystallize (ISO 4895:2014)
- EN ISO 4895:1999 Plastics - Liquid Epoxy Resins - Determination of Tendency to Crystallize
- EN ISO 2554:1998 Plastics - Unsaturated Polyester Resins - Determination of Hydroxyl Value
- EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004)
Lithuanian Standards Office , toughness of resin
- LST EN ISO 11402:2005 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004)
- LST EN ISO 11402:2005/AC:2006 Phenolic, amino and condensation resins - Determination of free-formaldehyde content (ISO 11402:2004)
- LST EN ISO 3673-2:2012 Plastics - Epoxy resins - Part 2: Preparation of test specimens and determination of properties of crosslinked epoxy resins (ISO 3673-2:2012)
- LST EN ISO 9944:2001 Plastics - Phenolic resins - Determination of electrical conductivity of resin extracts (ISO 9944:1990)
- LST EN ISO 9771:2001 Plastics - Phenolic resins - Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions (ISO 9771:1995)
General Administration of Quality Supervision, Inspection and Quarantine of the People‘s Republic of China, toughness of resin
- GB/T 24147-2009 Waterborne ultraviolet curable resin.Water soluble unsaturated polyester acrylate resin
- GB/T 22905-2008 Superabsorbent polymer for diaper
- GB/T 22875-2008 Superabsorbent polymer for santitary towel
- GB/T 1630.2-2023 Plastic epoxy resins Part 2: Specimen preparation and property determination of cross-linked epoxy resins
- GB/T 15022.9-2022 Resin based reactive compounds used for electrical insulation—Part 9:Resins for cable accessories
- GB/T 2567-2008 Test methods for properties of resin casting boby
- GB/T 2895-1982 Determination for acid value of unsaturated polyester resins
- GB/T 15022.4-2009 Resin based reactive compounds used for electrical insulation.Part 4:Unsaturated polyester based impregnating resins
- GB/T 32675-2016 Plastics.Phenolic resins.Determination of the pseudo-adiabatic temperature rise of liquid resols when cured under acid conditions
- GB/T 15022.3-2011 Resin based reactive compounds used for electrical insulation.Part 3:Unfilled epoxy resinous compounds
- GB/T 2568-1995 Test method for tensile properties of resin casting body
- GB/T 2569-1995 Test method for compressive properties of resin casting body
- GB/T 2570-1995 Test method for flexural properties of resin casting body
- GB/T 1303.4-2009 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes.Part 4:Requirements for rigid laminated sheets based on epoxy resins
- GB/T 1303.6-2009 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes.Part 6:Requirements for rigid laminated sheets based on phenolic resins
- GB/T 1303.7-2009 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes.Part 7:Requirements for rigid laminated sheets based on polyester resins
- GB/T 15022.5-2011 Resin based reactive compounds used for electrical insulation.Part 5:Quartz filled epoxy resinous compounds
- GB/T 1303.8-2009 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes.Part 8:Requirements for rigid laminated sheets based on silicone resins
- GB/T 5547-2007 Resin finishing agent.Determination of the viscosity
- GB/T 26735-2011 Glass fiber reinfoced thermosetting resin spray pipe
- GB/T 27808-2011 Saturated polyester resins for thermosetting powder coatings
- GB/T 1303.9-2009 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes.Part 9:Requirements for rigid laminated sheets based on polyimide resins
Professional Standard - Light Industry, toughness of resin
Standard Association of Australia (SAA), toughness of resin
ZA-SANS, toughness of resin
(U.S.) Ford Automotive Standards, toughness of resin
GM North America, toughness of resin
FI-SFS, toughness of resin
Hebei Provincial Standard of the People's Republic of China, toughness of resin
UY-UNIT, toughness of resin
中华人民共和国国家质量监督检验检疫总局、中国国家标准化管理委员会, toughness of resin
- GB/T 33323-2016 Plastics—Liquid phenolic resins—Determinaiton of water miscibility
- GB/T 34006-2017 Cardanol modified phenolic resin for composite material
- GB/T 1303.5-2017 Industrial rigid laminated sheets based on thermosetting resins for electrical purposes—Part 5: Requirements for rigid laminated sheets based on melamine resins
- GB/T 15022.7-2017 Resin based reactive compounds used for electrical insulation—Part 7: Epoxy-anhydride vacuum pressure impregnation(VPI) resin
- GB/T 15022.8-2017 Resin based reactive compounds used for electrical insulation— Part 8:Epoxy modified unsaturated polyester vacuum pressure impregnation (VPI) resin
Professional Standard - Petroleum, toughness of resin
- SY/T 6572-2003 Evaluation method of resin performance for sand control
Professional Standard - Machinery, toughness of resin
Jilin Provincial Standard of the People's Republic of China, toughness of resin
国家市场监督管理总局、中国国家标准化管理委员会, toughness of resin
International Federation of Trucks and Engines, toughness of resin
AR-IRAM, toughness of resin
YU-JUS, toughness of resin
- JUS G.S1.813-1991 Plastics.Epoxide resins and qlicidyl esters.Determination of inorqanic chlorine
- JUS G.S1.831-1991 Plastics.Polyester and epoxy casting resins.Determination of total volume skrinkage
- JUS G.S1.752-1991 Plastics. Liquid phenolic resins.Determination of water miscibility
- JUS N.A8.222-1993 Specification for solventless polymerisable resinous compounds used in electrical insulation - Specifications for individual materials - Unfilled epoxy resinous compounds
Professional Standard - Commodity Inspection, toughness of resin
- SN/T 3095-2012 Identification methods for primary plastic resins and recycled plastic resins
- SN/T 0560.1-1996 Determination of size of expandable polystyrene raw materials for import and export
- SN/T 2813-2011 Determination of extracts in melamine-formaldehyde resin, nylon resin and polycarbonate resin of polymer materials for export food contact materials
American Welding Society (AWS), toughness of resin
- WRC 577:2020 Constraint Effects on Fracture Toughness in the Ductile-Brittle Transition Region
- WRC 540:2014 Constraint Effects on Fracture Toughness in the Ductile-Brittle Transition Region
BELST, toughness of resin
- STB 1466-2004 Compositions protective modified epoxy. Specifications
国家林业和草原局, toughness of resin
GOSTR, toughness of resin
- GOST 29327-2017 Plastics. Liquid phenolic resins. Determination of water miscibility
KR-KS, toughness of resin
European Committee for Electrotechnical Standardization(CENELEC), toughness of resin
- EN IEC 60455-3-8:2021 Resin based reactive compounds used for electrical insulation - Part 3-8: Specifications for individual materials - Resins for cable accessories
- EN 60455-3-8:2013 Resin based reactive compounds used for electrical insulation - Part 3: Specifications for individual materials - Sheet 8: Resins for cable accessories
CO-ICONTEC, toughness of resin
Institute of Interconnecting and Packaging Electronic Circuits (IPC), toughness of resin
National Aeronautics and Space Administration (NASA), toughness of resin
Sichuan Provincial Standard of the People's Republic of China, toughness of resin
American Society of Mechanical Engineers (ASME), toughness of resin
- ASME NM.2-2020 Glass-Fiber-Reinforced Thermosetting-Resin Piping Systems
American National Standards Institute (ANSI), toughness of resin
- ASME NM.2-2022 Fiber-Reinforced Thermosetting-Resin Piping Systems
- ANSI/ASTM D3517:2011 Specification for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pressure Pipe
IN-BIS, toughness of resin
ES-UNE, toughness of resin
- UNE-EN 60455-3-8:2013 Resin based reactive compounds used for electrical insulation - Part 3: Specifications for individual materials - Sheet 8: Resins for cable accessories (Endorsed by AENOR in August of 2013.)
- UNE-EN IEC 60455-3-8:2021 Resin based reactive compounds used for electrical insulation - Part 3-8: Specifications for individual materials - Resins for cable accessories (Endorsed by Asociación Española de Normalización in September of 2021.)
The American Road & Transportation Builders Association, toughness of resin
Professional Standard - Building Materials, toughness of resin
- JC/T 552-2011 Filament-wound thermosetting resin pressured pipe
- JC 552-1994 Filament winding reinforced thermosetting resin pressure pipe
NEMA - National Electrical Manufacturers Association, toughness of resin
Military Standard of the People's Republic of China-General Armament Department, toughness of resin
- GJB 9266-2017 Specification for modified epoxy resin infusion sealing materials
CH-SNV, toughness of resin