83.080.10 热固性塑料 标准查询与下载



共找到 1195 条与 热固性塑料 相关的标准,共 80

本标准适用于流动长度变化范围较大的热固性模塑料流动固化性的测定。

Test method for rectangular flow cure properties of thermosetting moulding compounds

ICS
83.080.10
CCS
G31
发布
1985-10-17
实施
1986-07-01

本标准适用于热压成型的酚醛、氨基热固性模塑料,作为对同一类型的材料在加热加压条件下制备相同试样和编制试验报告的依据。

Preparation method for compression moulding of specimens of thermosetting moulding materials

ICS
83.080.10
CCS
G31
发布
1985-10-17
实施
1986-07-01

本标准规定了用丙酮在其沸点附近从磨细的酚醛模塑制品试样中,测定可抽提物数量的重量法。丙酮可溶物试验是一种测定由酚醛模塑料制成酚醛模塑制品相对固化度的方法。抽提过程应在指定条件下,于规定时间内进行。虽然测定了可溶物的大部分,但抽提作用不一定完全,其结果仅是一个比较的结果,因为抽提物常常含有未固化树脂以外的物质(如润滑剂、着色剂和增塑剂)。

Phenolic mouldings--Determination of acetone-soluble matter

ICS
83.080.10
CCS
G32
发布
1984-07-30
实施
1985-05-01

本标准规定了能用丙酮在其沸点附近从颗粒的酚醛模塑料中,测定抽提物数量的重量法。 本方法仅适用于以线型酚醛树脂为基材的模塑料,而不适用于以甲阶酚醛树脂为基材的模塑料, 因为后一类的树脂不能完全溶于丙酮。

Phenolic moulding materials--Determination of acetone soluble matter(apparent resin content of material in the unmoulded state)

ICS
83.080.10
CCS
G32
发布
1984-07-30
实施
1985-05-01

Standard Practice for Polyurethane Raw Materials: Polyurethane Foam Cup Test

ICS
83.080.10
CCS
发布
2024-02-01
实施

Determination of viscosity of thermosetting resins by rotational rheometer method

ICS
83.080.10
CCS
G31
发布
2023-12-20
实施
2024-07-01

Plastics — Determination of apparent density of moulding material that cannot be poured from a specified funnel

ICS
83.080.10
CCS
发布
2023-09
实施
2023-09

Plastics — Determination of apparent density of material that can be poured from a specified funnel

ICS
83.080.10
CCS
发布
2023-09
实施
2023-09

Plastics — Aminoplastic moulding materials — Determination of volatile matter

ICS
83.080.10
CCS
发布
2023-09
实施
2023-09

1   Scope This document specifies methods used to measure the water content of polyols employed as polyurethane raw materials. Method A is a manual amperometric method which has been included to better define the principles of the Karl Fischer measurement. Amperometric methods are applicable to a wide range of polyols , including those which have enough colour to obscure a visual end-point. Method B includes an automated amperometric procedure and an automated coulometric procedure. The coulometric procedure is an absolute method that does not require calibration and gives improved sensitivity compared with amperometric methods.

Plastics. Polyols for use in the production of polyurethanes. Determination of water content

ICS
83.080.10
CCS
发布
2023-08-31
实施
2023-08-31

Plastics. Polyols for use in the production of polyurethanes. Determination of degree of unsaturation by microtitration

ICS
83.080.10
CCS
发布
2023-07-31
实施
2023-07-31

Standard Test Method for Laboratory Measurement of Formaldehyde Evolved During the Curing of Melamine-Formaldehyde-Based Coatings

ICS
83.080.10
CCS
发布
2023-07-01
实施

Plastics — Polyols for use in the production of polyurethanes — Determination of water content

ICS
83.080.10
CCS
发布
2023-06
实施
2023-06

Plastics — Polyols for use in the production of polyurethanes — Determination of degree of unsaturation by microtitration

ICS
83.080.10
CCS
发布
2023-06
实施
2023-06

BS EN ISO 14900. Plastics. Polyols for use in the production of polyurethane. Determination of hydroxyl number

ICS
83.080.10
CCS
发布
2023-05-16
实施
2023-05-16

1.1 This specification2 covers polytetrafluoroethylene (PTFE) prepared by coagulation of a dispersion. These PTFE resins are homopolymers of tetrafluoroethylene or modified homopolymers containing not more than 1 % by weight of other fluoromonomers. The materials covered herein do not include mixtures of PTFE with additives such as colors, fillers, or plasticizers; nor do they include reprocessed or reground resin or any fabricated articles because the properties of such materials have been irreversibly changed when they were fibrillated or sintered. 1.2 The values stated in SI units as detailed in IEEE/ASTM SI-10 are to be regarded as standard. The values given in parentheses are for information only. 1.3 The following safety hazards caveat pertains only to the Specimen Preparation Section, Section 9, and the Test Methods Section, Section 10, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. See Warning note in 9.1.1 for a specific hazards statement. NOTE 1—Information in this specification is technically equivalent to related information in ISO 20568-1 and ISO 20568-2. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Specification for Polytetrafluoroethylene (PTFE) Resin Produced From Dispersion

ICS
83.080.10
CCS
发布
2023-05-01
实施

Plastics-Polyols for Use in the production of polyurethanes- Determination of degree of unsaturation value by using Iodine method

ICS
83.080.10
CCS
发布
2023-05
实施

1.1 This method covers the use of dynamic mechanical instrumentation for determination and reporting of the thermal advancement of cure behavior of thermosetting resin on an inert filler or fiber in a laboratory. It may also be used for determining the cure properties of resins without fillers or fibers. These encapsulated specimens are deformed in torsional shear using dynamic mechanical methods. 1.2 This method is intended to provide means for determining the cure behavior of thermosetting resins on fibers over a range of temperatures from room temperature to 250 °C by forced-constant amplitude techniques (in accordance with Practice D4065). Plots of complex modulus, complex viscosity, and damping ratio or tan delta as a function of time or temperature, or both, quantify the thermal advancement or cure characteristics of a resin or a resin on filler or fiber. 1.3 Test data obtained by this method is relevant and appropriate for optimizing cure cycles. 1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.4.1 Exception—The Fahrenheit temperature measurement in 10.1 is provided for information only and is not considered standard. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.6 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Test Method for Cure Behavior of Thermosetting Resins by Dynamic Mechanical Procedures using an Encapsulated Specimen Rheometer

ICS
83.080.10
CCS
发布
2023-04-01
实施

1.1 This test method measures the acidity, expressed as ppm of hydrochloric acid (HCl), in aromatic isocyanate or polyurethane prepolymer samples of below 100 ppm acidity. The test method is applicable to products derived from toluene diisocyanate and methylene di(phenylisocyanate) (see Note 1). Refer to Test Method D6099 for determination of acidity in moderateto high-acidity aromatic isocyanates. 1.2 The values stated in SI units are to be regarded as the standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. NOTE 1—This standard is equivalent to ISO 14898, Method B. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Test Method for Polyurethane Raw Materials: Determination of Acidity in Low-Acidity Aromatic Isocyanates and Polyurethane Prepolymers

ICS
83.080.10
CCS
发布
2023-03-01
实施

1.1 These test methods determine the total chlorine content of aromatic isocyanates used as polyurethane raw materials. The difference between the total chlorine content and the hydrolyzable chlorine content (see Test Method D4663) is a measure of the amount of chlorobenzene, o-dichlorobenzene, and other ring-substituted chlorinated products that are present. Both procedures are applicable to a variety of organic compounds but the amount of sample used is varied. (See Note 1.) 1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. NOTE 1—This standard is identical to ISO 26603. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Standard Test Methods for Polyurethane Raw Materials: Determination of Total Chlorine in Isocyanates

ICS
83.080.10
CCS
发布
2023-03-01
实施



Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号